Ask anyone who runs an aluminium workboat what keeps them busy. It will not be the engine. It will be the slow, quiet job of stopping the hull from eating itself.
Checking the anodes. Replacing the anodes. Inspecting the fittings. Finding the spot where the coating has lifted. Wondering, again, whether that hairline mark at the through hull is the start of something.
This is not bad luck and it is not bad building. It is chemistry, and it is doing exactly what it is supposed to do.
What is actually happening
Galvanic corrosion needs three things at the same time. Two different metals. An electrical connection between them. And an electrolyte, a liquid that lets ions move between the two.
Put a stainless fitting on an aluminium hull, drop the boat in the sea, and you have all three. Salt water is one of the best electrolytes there is. The two metals form a cell, a small battery you never asked for. One of them gives up electrons to the other. The one that gives is called the anode, and the anode is the one that dissolves.
Aluminium sits near the active end of the galvanic series, which is a polite way of saying it is usually the one that loses. That is also why aluminium is used to make sacrificial anodes. The material you built your hull from is the same material the industry uses when it wants something to corrode on purpose.
The further apart two metals sit on that series, the harder the reaction. Aluminium against stainless is a manageable pairing. Aluminium against copper or brass, in sea water, is not a pairing at all. It is a countdown.
What builders do about it
Quite a lot, and it works, up to a point.
You insulate. Every place where stainless meets aluminium gets a non conductive gasket, a sleeve, a washer. You coat both sides. You fit sacrificial anodes so that something cheap corrodes instead of something expensive. You design the electrical system so that stray current has nowhere to go, and you fit a galvanic isolator so the shore power in the marina does not quietly feed the reaction. Then you inspect all of it, on a schedule, forever.
None of this is exotic. Any decent yard will do it properly.
But look at what it is. It is a boat that needs a maintenance regime to stop it from failing. Every one of those measures can be skipped, forgotten, or done badly by whoever owns the boat after you. And the reaction never switches off. It only needs one place where the insulation failed, one bolt replaced with the wrong one, one bracket someone added later with the best of intentions.
Then comes the geography. Warmer, saltier water speeds the whole thing up. So does a busy marina full of shared electrical systems. So does a boat that sits still for weeks. Even damp air keeps a slow reaction going at the contact points of a boat that is out of the water entirely.
Why our hulls do not have this conversation
HDPE, or PEHD if you are reading this in French, is an engineering thermoplastic. It is an insulator. It does not conduct, so it cannot be the anode in a galvanic cell, and it cannot be the cathode either.
There is no potential difference between a polyethylene hull and the sea, because there is no potential at all. Take the metal out of the hull and the reaction has nothing to work with. No anodes on the hull. No coating on the hull to maintain. No inspection regime for the hull. No slow surprise in year six.
Let us be precise, because this audience notices when someone overstates a case. A Tideman is not a boat without metal. There is an engine, there are fittings, there is hardware, and metals in salt water still behave the way metals in salt water behave. Any sensible operator still looks after them.
What has gone is the largest metal object in the equation, permanently immersed, and everything you were doing to protect it.
What this means when you are a long way from a yard
Our boats work in places where nothing can be fixed. Ascension, halfway between Brazil and Africa, where a supply ship comes a few times a year and our boat is what gets it unloaded. The Falklands, where the fuel hose has to come ashore over the rocks because the observation posts run on generators. Greenland, where a customer drives across the ice with the boat behind a snowmobile once the water closes up.
There is no service network out there. No yard to haul out to. No coating shop.
That is where a hull that cannot corrode stops being a technical detail and becomes the reason the job gets done. Not because we are clever, but because we removed the problem instead of managing it.
We have built more than 400 HDPE boats. Some of them lead hard lives. Salvage crews run their bows into steel for a living, and after five years or so one comes back to us and we weld an extra plate where the material has worn away. That is wear and tear, and we can repair it, because you can weld this material back to what it was.
What has never brought a hull back here is corrosion. Not once. None of those hulls carries a sacrificial anode, because the hull has nothing to protect.
To be exact, because this reader will ask. Where a boat has a waterjet or a stern drive, those aluminium parts get an anode, as they should. And where you do see a small plate on the hull, it is not fighting corrosion at all. It is a grounding plate, an earth point that gives the electronics a clean zero in the water. The hull itself still has nothing to give away.
Salt water is going to keep doing what salt water does. The question is only whether you have given it something to work on.